Example of conventional grinding and polishing process常规研磨抛光处理工艺过程示例
| 1. | Before polishing, clean the surface to be polished with degreasing materials.抛光前将待抛光表面用脱脂材料清洗干净 |
| 2. | Apply an appropriate amount of polishing paste to the paint surface to be polished, and adjust the polishing machine speed取适量抛光膏涂于待抛光漆面上,调整抛光机转速 |
| 3. | Put the wool ball on the paint surface and then turn it on, the speed is 2500-3000r/min将羊毛球贴上漆面后再开机,转速2500-3000r/min
|
| 4. | First, fully wet the sponge and squeeze out the excess water; apply a small amount of glazing wax on the surface to be polished, put the sponge on the paint surface, then turn on the machine, rotate at 2500-3000r/min, and then press lightly for 3-5 seconds for glazing.先将海绵充分湿润,挤去多余水分;取少量上光蜡涂抹在待抛漆面上,将海绵贴上漆面后再开机,转速2500-3000r/min,再轻压3-5s进行上光处理
|