Body › Plastic panel information and repair › Repair
热固件塑料凹坑的维修 · T00386366

 Repair of plastic dents in thermal fixtures热固件塑料凹坑的维修

1. Clean and dry the parts to be repaired1. 清洗干燥待维修部件
2. Use a hot air blower to heat the dented area until the dent can be flattened with a suitable tool.2. 用热风机加热凹坑部位,直至可用合适的工具压平凹坑
3. Smooth the pitted area with sandpaper or emery paper3. 用砂纸或金刚砂纸打磨凹坑区域
4. Use detergent to clean the repaired area and wait for about 5 minutes to dry.4. 使用清洗剂清洗维修部位,等待5min左右晾干
5. Apply a thin layer of adhesive and wait for about 10 minutes to dry.5. 涂一层薄薄的粘结剂并等待10min左右晾干
6. Fill the uneven surface with adhesive and smooth it with a spatula6. 用粘结剂填充不平表面,用抹刀抹平
7. Use infrared lamp to accelerate the curing process, adjust the temperature to 60~70℃ (140~158ºF), and heat for about 15 minutes7. 用红外线灯加速固化过程,将温度调至60~70℃(140~158ºF),加热15min左右
8. Use sandpaper to polish the pits8. 用砂纸打磨凹坑部位
9. Remove dust and grinding debris9. 去除灰尘磨屑
10. Apply a thin layer of adhesive and wait for about 10 minutes to dry.10. 涂一层薄薄的粘结剂,等待10min左右晾干
11. Follow the paint repair procedure on the surface of the plastic parts to restore the paint surface11. 按塑料件表面的漆面修补程序恢复漆面